The Curie Temperature

A magnetised ferromagnetic component can lose its strong magnetic behaviour when heated, even though the metal remains solid. Has the heat destroyed the magnetic moments inside the material, or has it changed the way those moments organise themselves?

A magnetised ferromagnetic component can lose its strong magnetic behaviour when heated, even though the metal remains solid. Has the heat destroyed the magnetic moments inside the material, or has it changed the way those moments organise themselves?

The second explanation is correct. Above a particular temperature, thermal agitation disrupts the long-range alignment responsible for ferromagnetism. That temperature is called the Curie temperature.

Pure iron, for example, loses its spontaneous ferromagnetic ordering at approximately 1043 K, or 770°C. It is still solid at this temperature. The change is magnetic, not a melting process.

This article extends beyond the required NSW Year 11 Physics syllabus. Its starting point is the Electricity and magnetism material, particularly electrical power, energy transfer, and the law of conservation of energy. The Curie temperature itself is additional physics, not a required HSC assessment topic. Year 11 is the assumed starting point, not an assessment requirement.

01From electrical energy to thermal agitation

You already know that an electrical circuit can transfer energy into thermal energy.

When current passes through a resistor, the resistor dissipates electrical energy as heat. The rate of energy transfer is its electrical power:

\[ P=I^2R \]

where:

  • \(P\) is electrical power, measured in watts (W).
  • \(I\) is current, measured in amperes (A).
  • \(R\) is electrical resistance, measured in ohms (\(\Omega\)).

If the current and resistance remain constant, the electrical energy transferred over a time interval is:

\[ E=P\Delta t \]

Here, \(E\) is energy in joules (J), and \(\Delta t\) is the time in seconds (s).

The law of conservation of energy tells us that this energy does not disappear. It is transferred into the internal energy of the resistor and, through heating, potentially into surrounding materials.

This gives us a way to connect electricity with magnetism: an electrical heating process can raise the temperature of a ferromagnetic material until its magnetic properties change.

Make a prediction: If the current through a resistor doubles while its resistance stays constant, does the heating power double?

No. Since power depends on the square of current,

\[ P=(2I)^2R=4I^2R \]

The heating power quadruples.

That increase in thermal energy can have consequences beyond simply making a component hot.

Worked example: Calculating energy dissipated in a resistor

A heating element has a resistance of \(3.0\ \Omega\). A constant current of \(2.0\ \text{A}\) passes through it for five minutes.

Calculate the electrical energy dissipated by the element.

Step 1

\[ I=2.0\ \text{A} \]

\[ R=3.0\ \Omega \]

Convert the time into seconds:

\[ \Delta t=5\times60=300\ \text{s} \]

Step 2

Using \(P=I^2R\):

\[ P=(2.0)^2(3.0) \]

\[ P=12\ \text{W} \]

Step 3

\[ E=P\Delta t \]

\[ E=12\times300 \]

\[ E=3600\ \text{J} \]

Final answer:

\[ \boxed{E=3.6\ \text{kJ}} \]

The heating element dissipates 3.6 kJ of electrical energy as thermal energy over the five minutes.

Notice that this does not automatically mean a nearby magnetic sample receives all 3.6 kJ. Some energy may remain in the heating element or escape into the surroundings.

That distinction becomes important when predicting how quickly a magnetic material reaches its Curie temperature.

02Why does heating disrupt ferromagnetism?

To understand the Curie temperature, we need to look inside a ferromagnetic material.

Materials such as iron contain atoms with magnetic moments, which arise mainly from the magnetic properties of their electrons.

A magnetic moment describes the strength and direction of an individual atomic contribution to magnetism. You can initially picture each moment as a tiny magnetic arrow.

In a ferromagnetic material, neighbouring atomic moments tend to align parallel to one another. This produces a collective magnetic arrangement.

The important interaction responsible for this alignment is called the exchange interaction.

The role of the exchange interaction

The exchange interaction is a quantum-mechanical interaction between neighbouring electron states. In a ferromagnet, it favours parallel alignment of neighbouring magnetic moments.

It is not simply the ordinary magnetic attraction between tiny bar magnets. Its origin lies in quantum mechanics, particularly the behaviour of electron wavefunctions and the Pauli exclusion principle.

You do not need to calculate the exchange interaction to understand the Curie temperature. The key idea is that it favours an ordered arrangement of magnetic moments.

Consider a crowd in which people tend to face the same direction as their neighbours.

When the crowd is relatively undisturbed, groups of people can maintain a consistent orientation. Different groups might face different directions, but within each group there is a clear pattern.

Now imagine increasing the amount of random movement. Maintaining that coordinated arrangement becomes increasingly difficult.

This is a useful analogy for what happens to magnetic ordering as temperature increases.

The analogy has limits: electrons do not consciously coordinate their directions, and the alignment comes from a quantum-mechanical interaction rather than people copying one another.

Thermal agitation competes with magnetic ordering

Temperature is related to the average energy of particles and the thermal fluctuations within a material.

As temperature increases, thermal fluctuations become more significant. These fluctuations disturb the orientations of magnetic moments.

At relatively low temperatures, the exchange interaction can maintain long-range ferromagnetic ordering despite thermal fluctuations.

As temperature rises, the fluctuations become increasingly effective at disrupting that order.

Eventually, the material reaches a temperature at which stable long-range ferromagnetic ordering can no longer be maintained.

This is the physical origin of the Curie temperature.

An important detail is that heating does not simply switch off the exchange interaction. The interaction still exists, but thermal fluctuations prevent it from maintaining the collective ordered state.

The Curie temperature is therefore a collective transition, not a simple point at which the thermal energy of one atom exactly equals the exchange energy of one neighbouring pair.

03What exactly is the Curie temperature?

The Curie temperature, represented by \(T_C\), is the temperature at which a ferromagnetic material loses its spontaneous long-range magnetic ordering.

Below \(T_C\), the material can exhibit ferromagnetism without an externally applied magnetic field.

Above \(T_C\), the material becomes paramagnetic.

Let’s unpack what this means.

Below the Curie temperature: ferromagnetic ordering

Below \(T_C\), neighbouring magnetic moments maintain long-range parallel alignment.

A region in which magnetic moments are aligned in a common direction is called a magnetic domain.

Within each domain, the magnetic moments point in approximately the same direction.

However, different domains can point in different directions.

This explains something that initially seems contradictory: an iron object can be ferromagnetic but have almost no net magnetisation.

If its domains point in opposing directions, their magnetic contributions can cancel.

An unmagnetised iron object can therefore contain strongly ordered magnetic domains without producing a large external magnetic field.

Applying an external magnetic field can cause favourably oriented domains to grow, increasing the object’s net magnetisation.

Above the Curie temperature: paramagnetic behaviour

Above \(T_C\), thermal fluctuations disrupt long-range ferromagnetic ordering.

The magnetic moments are no longer locked into a common direction across the material.

The material becomes paramagnetic.

However, this does not mean that its atomic magnetic moments have disappeared.

If an external magnetic field is applied, the moments can still respond by becoming preferentially aligned with that field. This produces an induced magnetisation.

The response is generally much weaker than the strong collective response associated with ferromagnetism.

This distinction is essential:

  • Below \(T_C\), spontaneous ferromagnetic ordering is possible without an external field.
  • Above \(T_C\), there is no spontaneous ferromagnetic ordering, but an applied field can still produce magnetisation.

The spontaneous magnetisation is the intrinsic magnetic ordering that exists without an applied external field. We can represent it by \(M_{\mathrm{sp}}\).

Magnetisation, represented by \(M\), is the net magnetic dipole moment per unit volume. Its SI unit is amperes per metre (A/m).

For a simple ferromagnetic material in zero applied field, the spontaneous magnetisation approaches zero as the temperature approaches \(T_C\) from below.

Iron as a real example

For pure iron at approximately atmospheric pressure, the Curie temperature is:

\[ T_C=1043\ \text{K} \]

To convert this into degrees Celsius, subtract 273.15:

\[ \theta=1043-273.15 \]

\[ \theta\approx770^\circ\text{C} \]

This means:

  • Below approximately 770°C, iron can exhibit ferromagnetic ordering.
  • Above approximately 770°C, iron becomes paramagnetic.
  • At the transition, its spontaneous ferromagnetic ordering disappears.

Iron does not melt at its Curie temperature. Its melting point is approximately 1811 K, considerably higher.

The Curie temperature is specific to the material and its conditions. Different elements and alloys have different Curie temperatures, so the value for pure iron cannot simply be applied to every type of steel or permanent magnet.

04The difference between magnetic order and magnetisation

There is one misconception worth dealing with before attempting more difficult problems.

A student might test an iron sample with a compass. If the compass does not move, they might conclude that the iron is not ferromagnetic.

That conclusion is not necessarily correct.

An unmagnetised piece of iron can contain many ferromagnetic domains pointing in different directions. Their magnetic contributions can cancel, producing almost zero net magnetisation.

The individual domains are still ferromagnetically ordered.

Compare this with iron heated above its Curie temperature. Its long-range ferromagnetic ordering has genuinely disappeared.

The two samples might produce similar external magnetic readings, but their internal magnetic states are different.

PropertyBelow \(T_C\)Above \(T_C\)
Magnetic stateFerromagneticParamagnetic
Long-range orderingPresentAbsent
Spontaneous magnetisationPossibleZero
Response to an external fieldStrong collective responseWeaker induced response
Magnetic domainsPresentNo stable ferromagnetic domains

This is why the Curie temperature must be understood in terms of magnetic ordering, rather than simply whether an object attracts another object.

It is also worth separating this idea from temperature-dependent chemical spontaneity. Both topics involve temperature changing the balance between competing contributions, but the Curie transition concerns magnetic ordering and exchange interactions, not a direct application of Gibbs free energy. For the related HSC Chemistry foundation, see Temperature and Gibbs Spontaneity for HSC Chemistry.

05Applying the Curie temperature to heating calculations

We can now combine the circuit model with the magnetic model.

Suppose an electrical heating element is used to heat a ferromagnetic sample.

The electrical power determines the rate at which energy is dissipated. The sample’s mass and specific heat capacity determine how much energy is required to increase its temperature.

The relevant thermal energy equation is:

\[ Q=mc\Delta T \]

where:

  • \(Q\) is thermal energy transferred to the sample, in joules.
  • \(m\) is the sample’s mass, in kilograms.
  • \(c\) is its specific heat capacity, in J kg\(^{-1}\) K\(^{-1}\).
  • \(\Delta T\) is its temperature change, in kelvin.

For temperature differences, a change of 1 K is numerically equivalent to a change of 1°C.

The important decision is whether the sample actually reaches \(T_C\).

A heater might dissipate enough electrical energy to make a component extremely hot, but that does not automatically mean its Curie temperature has been reached.

We need to account for how much energy enters the sample.

Worked example: Heating a ferromagnetic alloy to its Curie temperature

A hypothetical ferromagnetic alloy has a Curie temperature of 320°C.

A sample has a mass of 0.20 kg and starts at 20°C. Its average specific heat capacity over this temperature range is 500 J kg\(^{-1}\) K\(^{-1}\).

A heating element with a resistance of \(4.0\ \Omega\) carries a constant current of \(3.0\ \text{A}\). Assume that 75% of the electrical energy dissipated by the element is transferred into the sample.

Calculate how long the heating element must operate for the sample to reach its Curie temperature.

Step 1

\[ \Delta T=320-20 \]

\[ \Delta T=300\ \text{K} \]

Step 2

Using \(Q=mc\Delta T\):

\[ Q=0.20\times500\times300 \]

\[ Q=30\,000\ \text{J} \]

The sample requires 30 kJ of thermal energy.

Step 3

\[ P=I^2R \]

\[ P=(3.0)^2(4.0) \]

\[ P=36\ \text{W} \]

Step 4

Only 75% of the electrical energy reaches the sample.

Therefore, the useful heating power is:

\[ P_{\mathrm{sample}}=0.75\times36 \]

\[ P_{\mathrm{sample}}=27\ \text{W} \]

Step 5

Since power is the rate of energy transfer:

\[ t=\frac{Q}{P_{\mathrm{sample}}} \]

\[ t=\frac{30\,000}{27} \]

\[ t\approx1111\ \text{s} \]

Converting into minutes:

\[ t=\frac{1111}{60} \]

\[ t\approx18.5\ \text{min} \]

Final answer:

\[ \boxed{t\approx18.5\ \text{minutes}} \]

The sample takes approximately 18.5 minutes to reach its Curie temperature under the stated assumptions.

At this point, its spontaneous ferromagnetic ordering disappears.

This is a simplified thermal model. It assumes a constant current, resistance, heating efficiency, and average specific heat capacity. Real materials can have a significant change in heat capacity near the Curie temperature, so accurate heating predictions require temperature-dependent material data.

The key physical connection is that electrical energy can increase thermal fluctuations enough to disrupt the magnetic ordering maintained by the exchange interaction.

06Questions and solutions

Question 1

A pure iron sample is heated to 800°C at approximately atmospheric pressure.

Determine whether the sample is ferromagnetic or paramagnetic at this temperature. Explain whether its atomic magnetic moments have disappeared.

Solution 1

The iron is paramagnetic at 800°C because this temperature is above its Curie temperature of approximately 770°C.

The Curie temperature marks the loss of spontaneous ferromagnetic ordering.

Above this temperature, thermal fluctuations prevent the magnetic moments from maintaining long-range parallel alignment.

However, the atomic magnetic moments have not simply disappeared. They can still respond to an applied magnetic field, producing a paramagnetic response.

The important distinction is that the material has lost its spontaneous ferromagnetic ordering, not every form of magnetic behaviour.

Question 2

An iron sample has a mass of 0.10 kg and an initial temperature of 300°C.

It is heated using an electrical element with a resistance of \(6.0\ \Omega\). A constant current of \(2.0\ \text{A}\) flows through the element for 600 seconds.

Assume that 70% of the electrical energy dissipated by the element is transferred into the iron sample.

The average specific heat capacity of the iron over this temperature interval is \(600\ \text{J kg}^{-1}\text{K}^{-1}\).

(a) Calculate the electrical power dissipated by the heating element.

(b) Calculate the thermal energy transferred into the iron.

(c) Estimate the final temperature of the sample.

(d) Determine whether the sample reaches its Curie temperature.

Solution 2

The sample reaches approximately 468°C, so it does not reach iron’s Curie temperature.

(a) Electrical power

Using:

\[ P=I^2R \]

Substitute:

\[ P=(2.0)^2(6.0) \]

\[ \boxed{P=24\ \text{W}} \]

The heating element dissipates 24 joules of electrical energy per second.

(b) Thermal energy transferred

First calculate the total electrical energy dissipated:

\[ E=P\Delta t \]

\[ E=24\times600 \]

\[ E=14\,400\ \text{J} \]

Only 70% reaches the sample:

\[ Q=0.70\times14\,400 \]

\[ \boxed{Q=10\,080\ \text{J}} \]

(c) Final temperature

Use the thermal energy equation:

\[ Q=mc\Delta T \]

Rearrange:

\[ \Delta T=\frac{Q}{mc} \]

Substitute:

\[ \Delta T= \frac{10\,080}{0.10\times600} \]

\[ \Delta T=168\ \text{K} \]

The final temperature is:

\[ T_f=300+168 \]

\[ \boxed{T_f=468^\circ\text{C}} \]

(d) Does the sample reach its Curie temperature?

No.

The Curie temperature of pure iron is approximately 770°C.

Since:

\[ 468^\circ\text{C}<770^\circ\text{C} \]

the sample remains below its Curie temperature.

It can therefore maintain spontaneous ferromagnetic ordering, although its magnetic properties will depend on its temperature and magnetic history.

A tempting mistake would be to use all 14,400 J in the thermal calculation. That ignores the 30% of electrical energy that escapes into the surroundings rather than entering the sample.

Conservation of energy still applies. We simply need to account for where the energy goes.

Question 3

Two iron bars are examined at approximately atmospheric pressure.

  • Bar A is at room temperature and has not been magnetised.
  • Bar B is heated to 800°C.

Neither bar produces a significant external magnetic field when measured without an applied field.

A student concludes that both bars must be paramagnetic.

Evaluate this conclusion. Explain the difference between the internal magnetic states of the two bars and describe one way to distinguish them experimentally.

Solution 3

The student’s conclusion is incorrect. Bar A is ferromagnetic but unmagnetised, whereas Bar B is paramagnetic.

The similar external magnetic readings do not mean the bars have the same internal magnetic structure.

Bar A: Room-temperature iron

Room temperature is well below iron’s Curie temperature.

Its atomic magnetic moments can form ferromagnetic domains. However, because the bar has not been magnetised, its domains can point in different directions.

Their magnetic contributions largely cancel, producing little net external magnetisation.

Bar B: Iron at 800°C

At 800°C, iron is above its Curie temperature.

Thermal fluctuations have disrupted the long-range ferromagnetic ordering.

The bar is paramagnetic, so it has no spontaneous ferromagnetic magnetisation in zero applied field.

How could we distinguish them?

Apply the same controlled external magnetic field to both bars and compare their responses.

Bar A can respond strongly because its domain walls can move and favourably oriented domains can grow.

Bar B responds through paramagnetic alignment of its magnetic moments. Its response is generally much weaker.

This is the crucial difference: Bar A contains ferromagnetic ordering that is hidden by domain cancellation, while Bar B has genuinely lost that ordering.

A measurement of net magnetisation alone is not always enough to identify the internal magnetic state.

Question 4

Two identical samples of a ferromagnetic alloy have a Curie temperature of 500 K.

Both samples are initially heated to 550 K.

They are then cooled to room temperature using two different procedures:

  • Sample A is cooled with no external magnetic field.
  • Sample B is cooled while a magnetic field is applied along its length.

The external field is removed after Sample B reaches room temperature.

Assume that the alloy has sufficient magnetic domain-wall pinning to retain a measurable remanent magnetisation after the applied field is removed. Also assume that the applied field is strong enough to favour domain alignment during cooling.

Predict which sample will have the greater net magnetisation at room temperature.

Does the other sample lack ferromagnetism?

Solution 4

Sample B will have the greater net magnetisation after the external field is removed. Sample A can still be ferromagnetic despite having almost zero net magnetisation.

The difference comes from the effect of the external magnetic field during the formation of magnetic domains.

Sample A: Cooling without an external field

At 550 K, Sample A is above its Curie temperature and has no spontaneous ferromagnetic ordering.

As it cools below 500 K, the exchange interaction begins to support long-range ferromagnetic ordering again.

However, there is no external field selecting a preferred direction for the magnetic domains.

Different domains can therefore form with different orientations. Their magnetic contributions can largely cancel.

The sample becomes ferromagnetic, but its net magnetisation can remain close to zero.

Sample B: Cooling in an external field

Sample B also loses its ferromagnetic ordering while above 500 K.

However, as it cools through the Curie temperature, the applied field favours magnetic moments and domains aligned along the field direction.

Domains favourably oriented with the field can grow at the expense of others.

When the sample reaches room temperature, removing the applied field does not necessarily remove its magnetisation.

Because the material has sufficient domain-wall pinning, it retains a remanent magnetisation.

This is the magnetisation remaining after an external magnetic field has been removed.

The important distinction is that the applied field does not create the exchange interaction or raise the Curie temperature. It influences the direction in which the ferromagnetic ordering develops.

Both samples are ferromagnetic at room temperature. Their different net magnetisations result from their different cooling histories.

Question 5

A ferromagnetic alloy has a Curie temperature of 500 K when no external magnetic field is applied.

A sample is heated using a resistive solenoid wrapped around it. The solenoid has a resistance of \(8.0\ \Omega\) and carries a constant current of \(1.5\ \text{A}\) for ten minutes.

The same current that heats the solenoid also generates a magnetic field along the sample.

Two trials are conducted.

In Trial A, a separate non-magnetic heater is used. No external magnetic field is applied during heating or cooling.

In Trial B, the current-carrying solenoid heats the sample. The current remains switched on while the sample cools back to 300 K. It is then switched off.

A magnetometer measures the sample’s net magnetisation. The solenoid’s own magnetic contribution has been accounted for in the measurements.

The following model readings are obtained:

MeasurementTrial ATrial B
Magnetisation at 525 KApproximately 0.000.04
Magnetisation at 300 K, after the heating equipment is switched off0.020.70

All magnetisation values are in arbitrary units.

Assume:

  • The two samples have identical composition and the same zero-field Curie temperature.
  • The solenoid’s field is weak enough not to substantially alter the material’s zero-field Curie temperature, but strong enough to produce a measurable paramagnetic response above that temperature.
  • The field is also strong enough to favour domain alignment while the sample cools below its Curie temperature.
  • The alloy retains measurable remanent magnetisation after the external field is removed.

(a) Calculate the electrical power dissipated by the solenoid and the total electrical energy dissipated over ten minutes.

(b) Trial B records a non-zero magnetisation at 525 K. Does this prove that the sample is still ferromagnetic or that its Curie temperature has increased? Explain.

(c) Explain why Trial B produces a much greater magnetisation at 300 K than Trial A, even though both samples have the same Curie temperature.

(d) Describe how you would modify the measurement procedure to investigate the zero-field Curie temperature without confusing field-induced magnetisation with spontaneous ferromagnetic ordering.

Solution 5

Trial B does not demonstrate an increase in the Curie temperature. Its non-zero magnetisation above 500 K is caused by the applied magnetic field, while its large room-temperature magnetisation results from field-biased domain formation during cooling.

The important complication is that the current-carrying solenoid has two effects: it transfers electrical energy into thermal energy, and it produces a magnetic field.

(a) Electrical power and energy

Calculate the power using:

\[ P=I^2R \]

Substitute:

\[ P=(1.5)^2(8.0) \]

\[ \boxed{P=18\ \text{W}} \]

Convert ten minutes into seconds:

\[ \Delta t=10\times60=600\ \text{s} \]

Calculate the total energy dissipated:

\[ E=P\Delta t \]

\[ E=18\times600 \]

\[ \boxed{E=10\,800\ \text{J}=10.8\ \text{kJ}} \]

The solenoid dissipates 10.8 kJ of electrical energy over the ten minutes.

This energy is available for heating the sample and surrounding apparatus. The calculation does not establish that all 10.8 kJ enters the sample.

(b) Why is the magnetisation non-zero at 525 K?

No, the non-zero magnetisation does not prove that the sample remains ferromagnetic.

The zero-field Curie temperature is 500 K, and the sample is at 525 K.

Therefore, it has lost its spontaneous ferromagnetic ordering.

However, the solenoid is still producing an external magnetic field.

Above the Curie temperature, the material is paramagnetic. Its magnetic moments can respond to an applied field by becoming preferentially aligned with it.

This produces a non-zero induced magnetisation.

The reading of 0.04 therefore represents a field-induced paramagnetic response, not evidence of surviving spontaneous ferromagnetic order.

A non-zero measured magnetisation does not automatically mean a material is ferromagnetic.

(c) Why is the room-temperature magnetisation much greater in Trial B?

The difference is caused by the magnetic field acting while the material cools through its Curie temperature.

In Trial A, the material cools without an external field.

When it passes below 500 K, ferromagnetic ordering develops, but the domains can form in different directions. Their contributions largely cancel, producing a small net magnetisation.

In Trial B, the solenoid remains energised throughout cooling.

As the material becomes ferromagnetic, the applied field favours domains aligned along its direction.

These domains grow, producing a larger net magnetisation.

Once the sample reaches 300 K, the current is switched off. However, the material retains some of its magnetisation because of magnetic hysteresis and domain-wall pinning.

This explains why Trial B produces a reading of 0.70 rather than approximately 0.02.

The samples have not acquired different Curie temperatures. They have acquired different magnetic histories.

(d) How should the zero-field Curie temperature be investigated?

The measurement should be performed with the external magnetic field reduced to zero, or with measurements repeated at progressively smaller fields and extrapolated towards zero field.

The important quantity is the spontaneous magnetisation, not simply the total magnetisation measured while an external field is present.

A suitable investigation would therefore:

  • Heat the sample while minimising external magnetic fields.
  • Measure its magnetic response as temperature increases.
  • Identify the disappearance of spontaneous ferromagnetic ordering.
  • Repeat measurements under controlled, decreasing applied fields if necessary, to separate field-induced effects from intrinsic magnetic ordering.

The zero-field Curie temperature remains 500 K.

The solenoid has not simply made the material ferromagnetic at a higher temperature. It has changed the magnetic conditions under which the sample was measured and cooled.

This is the deeper lesson: electrical heating and electromagnetic effects can occur simultaneously, so an experiment that changes temperature may also change the magnetic field acting on the sample.

07Where this leads next

The Curie temperature explains why a ferromagnetic material can lose its spontaneous magnetic ordering when heated, and why cooling does not necessarily restore its original net magnetisation.

The next useful concept is magnetic hysteresis.

Hysteresis explains why a material’s magnetisation depends on its previous magnetic history. It introduces remanent magnetisation, coercivity, and the behaviour that allows some materials to act as permanent magnets.

Together, the Curie temperature and magnetic hysteresis explain two different ways temperature and magnetic fields influence the behaviour of real magnetic materials.

08Scientific references

The following university teaching materials and scientific references support the physical models and material properties discussed in this article.