Battery State of Health
A lithium-ion battery can read 3.8 V after resting and still shut down when asked to deliver a burst of current. Another battery might deliver that burst perfectly well but run out much sooner than it did when new.
A lithium-ion battery can read 3.8 V after resting and still shut down when asked to deliver a burst of current. Another battery might deliver that burst perfectly well but run out much sooner than it did when new. Both batteries are ageing, but they are experiencing different forms of degradation.
Suppose two batteries have exactly the same voltage after resting. Does that mean they have the same battery health? Not necessarily. A voltage reading tells you something about the battery’s electrical condition at that moment. It does not tell you how much charge the battery can still store or how effectively it can deliver that charge.
These are two important parts of battery state of health (SOH): capacity loss and internal resistance growth.
This article goes beyond the required Chemistry syllabus. It uses concepts from the Year 12 Chemistry 11-12 Syllabus (2025), particularly Applying chemical ideas, as a foundation. Understanding battery state of health is extension learning, not an additional HSC assessment requirement. NESA schedules implementation of the 2025 syllabus from 2028, with the first HSC examination in 2029.
All numerical values in the worked examples and practice questions are illustrative.
Due to technical limitations, this figure may display incorrectly or contain inaccuracies. Please check key details against your course materials.
01A useful syllabus connection: AES and flame tests
Before examining battery health, it is worth revisiting an analytical chemistry distinction from Applying chemical ideas: atomic emission spectroscopy (AES) and flame tests.
Both techniques use the emission of light by excited atoms to identify elements.
When atoms absorb energy, their electrons can move into higher energy levels. These excited states are unstable. As electrons return to lower energy levels, they release energy as electromagnetic radiation.
The wavelengths of this emitted light depend on the energy differences between the allowed electron energy levels.
Different elements have different electron configurations and energy levels, so they produce characteristic emission spectra.
Flame tests: identifying elements by colour
A flame test is a simple qualitative method of elemental analysis.
A small sample of a suitable metal salt is heated in a flame. The sample is vaporised, and some of the resulting atoms become excited. As their electrons return to lower energy levels, they emit light.
If the emitted wavelengths fall within the visible region, the flame appears coloured.
For example:
- Sodium produces a characteristic intense yellow emission.
- Potassium produces a lilac emission.
- Copper compounds can produce blue-green emissions.
- Calcium produces an orange-red emission.
A flame test provides an indication of which elements may be present. However, the human eye sees the combined visible light rather than separating every individual wavelength.
This creates problems when samples contain mixtures. A strong sodium emission, for example, can overwhelm weaker emissions from other elements.
Flame tests are therefore useful for qualitative identification, but they are not reliable methods for determining the concentration of each element in a mixture.
Atomic emission spectroscopy: measuring emitted wavelengths and intensity
Atomic emission spectroscopy takes the same general emission principle further.
Instead of relying on the human eye to judge the flame colour, an instrument separates the emitted light into its individual wavelengths and measures their intensities.
The wavelengths help identify the elements present. The intensity of a selected emission line can be compared with calibration standards to determine the concentration of that element.
Depending on the instrument, the sample atoms may be excited using a flame or a high-temperature plasma.
The important difference is that instrumented AES provides much more detailed information than a visual flame test.
| Feature | Flame test | Atomic emission spectroscopy |
|---|---|---|
| Principle | Excited atoms emit light | Excited atoms emit light |
| Observation | Overall visible flame colour | Individual emission wavelengths and intensities |
| Element identification | Qualitative | Qualitative |
| Concentration measurement | Not reliably quantitative | Quantitative with suitable calibration |
| Main limitation | Overlapping colours and mixtures | Requires specialised equipment and appropriate calibration |
The NESA Chemistry 2025 glossary describes AES as an analytical technique for determining the concentration of metal ions in a sample using emitted light.
A useful scientific detail: the visible emission in a conventional flame test generally comes from excited neutral atoms formed after the salt is vaporised, rather than directly from the metal ions originally dissolved in the sample. This distinction is discussed in the 2025 Journal of Chemical Education paper, Misconceptions and Insights about Flame Tests.
Why does this matter for battery health?
Imagine analysing a sample taken from a professionally prepared lithium-ion battery experiment.
AES could help identify and measure transition metals present in the sample, including metals associated with the battery’s electrode materials.
This could provide evidence about changes in the battery’s chemical composition.
However, knowing which elements are present does not tell us how much electrical charge the battery can deliver.
That requires a different type of measurement.
This is the distinction to remember:
- AES and flame tests investigate elemental composition.
- Battery capacity and resistance tests investigate electrical performance.
We will use this distinction throughout the article.
02Understanding the chemistry inside a lithium-ion battery
To understand why battery health changes, first consider how a rechargeable lithium-ion cell operates.
A typical lithium-ion battery contains:
- A negative electrode, commonly made from graphite.
- A positive electrode, made from a lithium-containing material.
- An electrolyte that allows lithium ions to move between the electrodes.
- A separator that prevents direct electronic contact between the electrodes while allowing ions to pass through.
Different lithium-ion battery chemistries use different electrode materials. The following explanation uses a common graphite-based cell as its model.
What happens during discharge?
When a battery powers a device, a spontaneous redox reaction takes place.
At the negative electrode, oxidation occurs. Lithium leaves the graphite structure as lithium ions, releasing electrons.
The lithium ions travel through the electrolyte towards the positive electrode.
Meanwhile, the electrons travel through the external circuit, providing electrical energy to the connected device.
At the positive electrode, reduction occurs as lithium ions and electrons participate in the electrode reaction.
The two pathways are important:
- Lithium ions move through the battery’s electrolyte.
- Electrons move through the external electrical circuit.
During charging, an external power source drives the reactions in the opposite direction.
A new battery can repeat these reactions many times.
However, repeated charging, discharging, and storage gradually change the electrode materials and the interfaces between the electrodes and electrolyte.
Some changes reduce the amount of charge the battery can deliver. Others make it harder for the battery to deliver charge quickly.
These are related, but different, forms of degradation.
03What does battery state of health actually measure?
State of health describes how a battery’s performance compares with a defined reference condition, usually its condition when new.
It is important not to confuse state of health with state of charge.
State of charge (SOC) describes how much charge is currently available relative to the battery’s present usable capacity.
State of health (SOH) describes how the battery’s performance has changed compared with its original or reference condition.
For example, an aged battery could be at 100% SOC while having only 80% of its original capacity.
It is completely charged relative to what it can currently hold, but it cannot store as much charge as when it was new.
Two different indicators of battery degradation
The two indicators we are investigating are:
- Capacity-based state of health.
- Resistance growth.
| Property | Capacity loss | Resistance growth |
|---|---|---|
| What changes? | Amount of charge the battery can deliver | Opposition to current flowing through the battery |
| Main consequence | Reduced energy available and shorter runtime | Greater voltage drop and reduced power capability |
| Typical observation | Battery runs out sooner | Battery struggles under high electrical demand |
| Common measurement | Controlled charge-discharge test | Current pulse test or impedance measurement |
| Main concern | How much charge remains usable? | How effectively can that charge be delivered? |
Think of a water tank connected to a pipe.
The capacity of the battery is loosely comparable to the amount of water the tank can hold. Resistance is loosely comparable to how difficult it is for water to flow through the pipe.
A smaller tank runs out sooner. A narrower pipe restricts how quickly water can be delivered.
The analogy is useful, but it is not exact. A battery is an electrochemical system, not a tank of stored liquid. Its capacity and resistance are influenced by interacting chemical reactions and transport processes.
A battery can therefore retain substantial capacity while experiencing serious resistance growth.
It can also lose capacity without experiencing an equally large increase in resistance.
There is no single universal SOH percentage that captures every aspect of battery performance. Different applications may prioritise capacity, energy, resistance, or power. Researchers commonly consider multiple health indicators rather than relying on one measurement.
A detailed discussion of these different definitions appears in Su, Xu, and Dong’s 2024 review, State-of-health estimation of lithium-ion batteries.
04Capacity loss: when a battery stores less usable charge
Battery capacity describes the amount of electrical charge that can be delivered between specified charging and discharging limits.
It is commonly measured in ampere-hours (Ah).
Suppose a new battery has a measured capacity of 3.0 Ah.
If it can deliver a current of 1.0 A for 3.0 hours under the specified test conditions, its delivered charge is:
\[ Q=It \]
where:
- \(Q\) is the delivered charge in ampere-hours (Ah).
- \(I\) is the discharge current in amperes (A).
- \(t\) is the discharge time in hours (h).
For a changing current, capacity is calculated by integrating current over time:
\[ Q=\int I\,\mathrm{d}t \]
This process of measuring and adding the charge transferred over time is called coulomb counting.
How is capacity measured?
In a controlled laboratory test, a battery is charged using a specified charging procedure.
It is then discharged at a controlled current until it reaches its specified lower voltage limit.
The total charge delivered during this discharge is recorded.
For a meaningful comparison, the new and aged batteries must be tested using the same relevant conditions, including:
- Temperature.
- Discharge current.
- Upper and lower voltage limits.
- Charging procedure.
- Measurement equipment and protocol.
Why are these conditions important?
Because the measured capacity depends partly on how the battery is tested.
For example, a battery discharged at a high current may reach its lower voltage limit earlier than the same battery discharged at a low current.
This means that the measured capacity is not completely independent of discharge rate.
Experimental studies have demonstrated the effects of discharge current and temperature on the measured capacity of lithium-ion cells. See the open-access study, Experimental data of lithium-ion batteries under galvanostatic discharge tests at different rates and temperatures.
Calculating capacity-based SOH
For a battery with a measured initial reference capacity, capacity-based state of health is:
\[ \mathrm{SOH}_{Q} = \frac{Q_{\mathrm{now}}} {Q_{\mathrm{ref}}} \times 100\% \]
where:
- \(\mathrm{SOH}_{Q}\) is capacity-based state of health.
- \(Q_{\mathrm{now}}\) is the battery’s currently measured capacity.
- \(Q_{\mathrm{ref}}\) is its initial reference capacity.
For this comparison, assume both capacities were measured using the same controlled test procedure.
The percentage capacity fade is:
\[ \text{Capacity fade} = 100\%-\mathrm{SOH}_{Q} \]
Worked example: calculate capacity-based state of health
A lithium-ion battery originally had a measured capacity of 3.20 Ah. After ageing, a controlled discharge test measures its capacity as 2.72 Ah.
Calculate its capacity-based SOH and percentage capacity fade.
Step 1
\[ Q_{\mathrm{ref}}=3.20\ \mathrm{Ah} \]
\[ Q_{\mathrm{now}}=2.72\ \mathrm{Ah} \]
Step 2
\[ \mathrm{SOH}_{Q} = \frac{Q_{\mathrm{now}}} {Q_{\mathrm{ref}}} \times100\% \]
Step 3
\[ \mathrm{SOH}_{Q} = \frac{2.72}{3.20} \times100\% \]
\[ \mathrm{SOH}_{Q}=85\% \]
Step 4
\[ \text{Capacity fade}=100-85 \]
\[ \boxed{\text{Capacity fade}=15\%} \]
The battery retains 85% of its original measured capacity under the specified test conditions.
This does not mean that exactly 15% of its lithium atoms have disappeared. It means that the amount of charge it can deliver under the reference test has decreased by 15%.
One final distinction matters: capacity in Ah measures electrical charge, not energy directly. The energy delivered also depends on the voltage throughout the discharge.
For batteries of the same chemistry and similar voltage profiles, capacity is a useful indicator of runtime. However, it does not describe the entire performance of the battery.
That brings us to the second indicator.
05Resistance growth: when a battery struggles to deliver current
Imagine two batteries with the same capacity.
Both can theoretically deliver 3.0 Ah under the same low-rate test.
However, when a device demands a large current, one battery experiences a much greater drop in terminal voltage.
Why?
Because its internal resistance is higher.
What is internal resistance?
Internal resistance describes the opposition to current flow within a battery.
It represents several contributions, including:
- Resistance within the electrodes and current collectors.
- Resistance to ion movement through the electrolyte and electrode interfaces.
- Resistance associated with interfacial reactions and charge-transfer processes.
- Additional effects caused by concentration gradients and electrochemical polarisation.
A real lithium-ion cell does not behave like one perfectly fixed resistor. Its effective resistance depends on temperature, state of charge, current, and the timescale over which it is measured.
However, a simple electrical model is useful for understanding the main effect.
During discharge:
\[ V_{\mathrm{load}} \approx V_{\mathrm{OCV}}-IR_{\mathrm{int}} \]
where:
- \(V_{\mathrm{load}}\) is the terminal voltage while the battery supplies current.
- \(V_{\mathrm{OCV}}\) is its open-circuit voltage, measured with no current flowing after an appropriate rest period.
- \(I\) is the discharge current, taken as positive.
- \(R_{\mathrm{int}}\) is the effective internal resistance.
The equation tells us something important.
As internal resistance increases, the voltage lost inside the battery increases for the same discharge current.
This means the voltage available to the external device decreases.
Measuring resistance using a current pulse
One way to estimate internal resistance is to apply a short, controlled current pulse and measure the voltage response.
The current changes, and the battery’s terminal voltage changes in response.
An approximate pulse resistance is calculated using:
\[ R_{\mathrm{pulse}} = \frac{|\Delta V|}{|\Delta I|} \]
where:
- \(R_{\mathrm{pulse}}\) is the apparent resistance measured during the pulse, in ohms (\(\Omega\)).
- \(\Delta V\) is the magnitude of the voltage change, in volts (V).
- \(\Delta I\) is the magnitude of the current change, in amperes (A).
The absolute values are used so that the calculated resistance is positive.
The measurement must use comparable conditions. In particular, the batteries should have the same chemistry, temperature, state of charge, and pulse duration.
A 10-second pulse measurement is not necessarily equal to a 1-second pulse measurement because slower electrochemical processes contribute to the voltage response.
Worked example: compare pulse resistance in a new and aged battery
A new lithium-ion cell is tested using a 10-second discharge pulse.
Its voltage decreases from 3.90 V to 3.82 V when the current increases from 0 A to 2.0 A.
An aged cell, tested at the same temperature and state of charge, experiences a voltage decrease from 3.90 V to 3.70 V under the same pulse.
Calculate the apparent pulse resistance of each cell and compare their resistive heating at 2.0 A.
Step 1
\[ \Delta V=3.90-3.82=0.08\ \mathrm{V} \]
\[ \Delta I=2.0-0=2.0\ \mathrm{A} \]
Step 2
\[ R_{\mathrm{new}} = \frac{0.08}{2.0} \]
\[ \boxed{R_{\mathrm{new}}=0.040\ \Omega} \]
Step 3
\[ \Delta V=3.90-3.70 \]
\[ \Delta V=0.20\ \mathrm{V} \]
Its current change is still 2.0 A.
Therefore:
\[ R_{\mathrm{aged}} = \frac{0.20}{2.0} \]
\[ \boxed{R_{\mathrm{aged}}=0.100\ \Omega} \]
Step 4
\[ \%\text{ increase} = \frac{R_{\mathrm{aged}}-R_{\mathrm{new}}} {R_{\mathrm{new}}} \times100\% \]
\[ = \frac{0.100-0.040}{0.040} \times100\% \]
\[ \boxed{150\%} \]
The aged cell has 2.5 times the measured pulse resistance of the new cell.
Step 5
The simplified relationship for resistive heating is:
\[ P_{\mathrm{heat}}=I^2R \]
where \(P_{\mathrm{heat}}\) is the electrical power dissipated as heat, in watts (W).
For the new cell:
\[ P_{\mathrm{new}}=2.0^2\times0.040 \]
\[ P_{\mathrm{new}}=0.16\ \mathrm{W} \]
For the aged cell:
\[ P_{\mathrm{aged}}=2.0^2\times0.100 \]
\[ P_{\mathrm{aged}}=0.40\ \mathrm{W} \]
The aged cell dissipates 2.5 times as much power as heat at the same current under this simplified model.
This is why resistance growth matters.
The battery might still retain a substantial amount of its original capacity, but it may struggle to supply high currents without excessive voltage sag and heating.
The pulse resistance is an effective measurement, not a complete description of every process inside the battery.
06Why do battery capacity and resistance change?
The interesting part is that capacity loss and resistance growth are often caused by overlapping chemical and physical changes.
To understand this, we need to distinguish between a degradation mechanism and its electrical consequences.
A degradation mechanism is the physical or chemical process occurring inside the cell.
A degradation outcome is the measurable change in battery performance.
Three important degradation processes help explain the relationship.
1. Growth of the solid-electrolyte interphase
The solid-electrolyte interphase (SEI) is a thin layer that forms on the surface of the negative electrode in many lithium-ion batteries.
It develops because the electrolyte is not completely stable at the operating potential of the lithiated graphite electrode.
Some electrolyte components undergo reduction reactions, producing compounds that deposit on the electrode surface.
This layer is not automatically harmful.
In fact, a stable SEI is important because it helps prevent continuous decomposition of the electrolyte.
The problem is continued growth.
As the SEI becomes thicker, two things can happen.
First, lithium becomes trapped in compounds within the SEI. That lithium is no longer available to participate in the normal charging and discharging reactions.
This reduces the amount of cyclable lithium in the cell.
The result is capacity loss.
Second, the SEI is less favourable for ion transport than the surrounding electrolyte. A thicker interphase can make lithium-ion movement more difficult.
The result is increased internal resistance.
Notice the connection: the same degradation process can contribute to both capacity fade and resistance growth.
The relationship between SEI growth, lithium inventory loss, and impedance increase is discussed in the Royal Society of Chemistry review, Lithium ion battery degradation: what you need to know.
2. Loss of active electrode material
Another form of degradation is loss of active material.
Electrode particles can develop cracks during repeated expansion and contraction as lithium enters and leaves their structures.
Some particles may lose electrical contact with the conductive network.
Others may become structurally damaged or chemically altered.
What happens to battery capacity?
If less electrode material remains available for electrochemical reactions, less lithium can be stored and released during normal operation.
This reduces the usable capacity.
There may also be an increase in resistance if the damage disrupts electrical connections or makes ion transport more difficult.
However, active material loss does not necessarily produce the same resistance increase in every cell.
3. Electrolyte degradation and lithium plating
The electrolyte provides the pathway through which lithium ions move between the electrodes.
If electrolyte is consumed, decomposed, or redistributed, ion transport can become less effective.
This can increase resistance and contribute to the isolation of active electrode material.
Another important mechanism is lithium plating.
During certain charging conditions, particularly when charging is too fast for the available ion-transport and insertion processes or when the cell is sufficiently cold, metallic lithium can deposit on the negative electrode instead of entering the graphite structure.
Some plated lithium may be recoverable, but some can react with the electrolyte or become electrically isolated.
These side reactions can consume cyclable lithium and contribute to capacity loss and further resistance growth.
Lithium plating can also create serious safety concerns, including conditions that may lead to internal short circuits.
These are complex internal degradation processes, not reactions that should be investigated by dismantling or experimentally stressing consumer batteries.
The important relationship
The main point is that capacity loss and resistance growth are related outcomes, but they are not interchangeable measurements.
| Degradation process | Possible effect on capacity | Possible effect on resistance |
|---|---|---|
| Continued SEI growth | Loss of cyclable lithium | Increased interfacial resistance |
| Loss of active material | Fewer available storage sites | Possible loss of electrical contact |
| Electrolyte depletion | Reduced usable active material | More difficult ion transport |
| Lithium plating | Loss of cyclable lithium through side reactions | Increased impedance and transport limitations |
These mechanisms can occur simultaneously and influence each other.
The result is that two batteries with similar capacity retention may have very different internal resistance.
Likewise, two batteries with similar pulse resistance may have different remaining capacities.
This is why battery SOH should not be reduced to a single measurement without explaining what that measurement represents.
07Why one voltage reading cannot diagnose battery health
We can now return to the original problem.
A battery voltage is useful information, but it is not a complete diagnosis.
The key is to distinguish open-circuit voltage from terminal voltage under load.
Open-circuit voltage
Open-circuit voltage (OCV) is the voltage measured when no external current is flowing.
After a suitable rest period, the voltage approaches the cell’s equilibrium voltage.
For a given battery chemistry, OCV is related to state of charge.
However, this relationship is not always simple.
It can depend on:
- The battery’s chemistry.
- Its temperature.
- Its ageing condition.
- Whether it was previously charging or discharging.
- How long it has been resting.
For example, lithium iron phosphate batteries can have a relatively flat OCV-versus-SOC relationship across a broad middle range of charge.
This makes it difficult to determine the exact SOC from one voltage measurement.
Research by Farmann and Sauer also demonstrates that temperature, ageing, and previous battery history influence OCV behaviour in lithium-ion cells.
See their study, A study on the dependency of the open-circuit voltage on temperature and actual aging state of lithium-ion batteries.
Terminal voltage under load
When current flows, the terminal voltage differs from the open-circuit voltage.
Recall the simplified relationship:
\[ V_{\mathrm{load}} \approx V_{\mathrm{OCV}}-IR_{\mathrm{int}} \]
A high discharge current produces a greater voltage drop across the battery’s internal resistance.
An aged battery with increased resistance may therefore show a much lower terminal voltage under load than a new battery at a similar state of charge.
When the load is removed, the voltage can recover.
Part of this recovery is immediate, as the ohmic voltage drop disappears. Further recovery occurs as concentration gradients and electrochemical polarisation relax inside the cell.
The battery has not magically recharged itself during the rest period. Its internal electrochemical conditions have redistributed.
What could a low voltage actually mean?
A low terminal voltage could indicate:
- A low state of charge.
- A large discharge current.
- Low operating temperature.
- Increased internal resistance.
- A battery fault or other abnormal operating condition.
A normal-looking rested voltage does not prove that the battery retains its original capacity.
Likewise, a low voltage under load does not automatically prove that the battery has lost a large percentage of its capacity.
A battery management system (BMS) therefore uses information from voltage, current, temperature, and operating history to estimate battery condition.
It may also use mathematical models and other diagnostic indicators.
For a more complete assessment, two particularly useful measurements are:
| Diagnostic method | What it investigates | Main limitation |
|---|---|---|
| Controlled discharge test | Available charge capacity | Takes time and depends on test conditions |
| Current pulse test | Effective internal resistance and voltage response | Sensitive to SOC, temperature, and pulse duration |
| Electrochemical impedance spectroscopy (EIS) | Frequency-dependent electrical response and different contributions to impedance | Requires more specialised equipment and model interpretation |
EIS is particularly useful when investigating how different electrochemical processes contribute to resistance changes. It is an extension of the same diagnostic idea, but uses small alternating electrical signals across a range of frequencies.
08Questions and solutions
The following questions move from basic capacity calculations to more demanding battery-diagnosis problems.
All data are hypothetical and supplied specifically for these questions.
Question 1
A lithium-ion battery originally has a measured capacity of 4.0 Ah.
After ageing, a controlled discharge test measures its capacity as 3.2 Ah.
Calculate:
a) Its capacity-based state of health.
b) Its percentage capacity fade.
Solution 1
The battery has a capacity-based SOH of 80% and a capacity fade of 20%.
The capacity-based SOH equation is:
\[ \mathrm{SOH}_{Q} = \frac{Q_{\mathrm{now}}} {Q_{\mathrm{ref}}} \times100\% \]
Part a: Calculate SOH
Substitute the measured capacities:
\[ \mathrm{SOH}_{Q} = \frac{3.2}{4.0} \times100\% \]
\[ \boxed{\mathrm{SOH}_{Q}=80\%} \]
Part b: Calculate capacity fade
\[ \text{Capacity fade} = 100\%-80\% \]
\[ \boxed{\text{Capacity fade}=20\%} \]
The battery can deliver 80% of its original measured charge capacity under the specified test conditions.
This result does not establish how much its internal resistance has changed. A separate electrical measurement is needed to investigate that.
Question 2
A lithium-ion cell originally has an internal resistance of 20 mΩ.
After ageing, its measured internal resistance increases to 70 mΩ.
Assume that:
- Both measurements were taken at the same temperature and state of charge.
- The pulse duration was identical.
- The battery supplies a constant discharge current of 5.0 A.
- The simplified ohmic model is valid for this comparison.
Calculate:
a) The percentage increase in internal resistance.
b) The additional voltage drop caused by the increase in resistance at 5.0 A.
c) The additional power dissipated as heat at this current.
Explain why a capacity-based SOH of 92% would not rule out this degradation.
Solution 2
The internal resistance has increased by 250%, producing an additional voltage drop of 0.25 V and an additional resistive power loss of 1.25 W at 5.0 A.
Part a: Calculate resistance growth
First convert milliohms into ohms.
\[ R_{\mathrm{ref}}=0.020\ \Omega \]
\[ R_{\mathrm{now}}=0.070\ \Omega \]
Use:
\[ \%\text{ increase} = \frac{R_{\mathrm{now}}-R_{\mathrm{ref}}} {R_{\mathrm{ref}}} \times100\% \]
Substitute:
\[ = \frac{0.070-0.020}{0.020} \times100\% \]
\[ \boxed{250\%} \]
The aged battery has 3.5 times its original resistance.
Part b: Calculate the additional voltage drop
The additional resistance is:
\[ \Delta R=0.070-0.020 \]
\[ \Delta R=0.050\ \Omega \]
Using the simplified voltage-drop relationship:
\[ \Delta V=I\Delta R \]
\[ =5.0\times0.050 \]
\[ \boxed{\Delta V=0.25\ \mathrm{V}} \]
The aged cell loses an additional 0.25 V internally at the same current.
Part c: Calculate additional heating
The resistive power relationship is:
\[ P_{\mathrm{heat}}=I^2R \]
Therefore, the additional power loss is:
\[ \Delta P=I^2\Delta R \]
\[ =5.0^2\times0.050 \]
\[ \boxed{\Delta P=1.25\ \mathrm{W}} \]
Why doesn’t 92% capacity SOH rule this out?
Capacity and resistance measure different aspects of battery performance.
A capacity-based SOH of 92% indicates that the battery retains 92% of its reference charge capacity.
It does not establish that the battery can deliver that charge at its original power capability.
The battery may still store most of its original charge while experiencing substantial resistance growth.
This is particularly important in devices that require high currents, such as electric vehicles and power tools.
Question 3
Two lithium-ion batteries have the same original reference capacity of 3.00 Ah and the same initial pulse resistance of 25 mΩ.
After ageing, their measured properties are:
| Property | Battery A | Battery B |
|---|---|---|
| Current capacity | 2.40 Ah | 2.82 Ah |
| Current pulse resistance | 30 mΩ | 75 mΩ |
| Reference capacity | 3.00 Ah | 3.00 Ah |
| Reference pulse resistance | 25 mΩ | 25 mΩ |
Assume both batteries have the same chemistry and similar voltage profiles.
a) Calculate the capacity-based SOH of each battery.
b) Calculate the percentage increase in pulse resistance of each battery.
c) Battery A is being considered for a high-power electric motor that requires short bursts of high current. Battery B is being considered for a low-power monitoring device that requires long operating periods.
Which battery is the more suitable choice for each application? Justify your decisions.
Solution 3
Battery B retains more capacity, but Battery A has substantially lower internal resistance. Battery B is therefore the better candidate for the low-power application, while Battery A is the better candidate for the high-power application under the stated assumptions.
Part a: Calculate capacity-based SOH
For Battery A:
\[ \mathrm{SOH}_{Q,A} = \frac{2.40}{3.00}\times100\% \]
\[ \boxed{\mathrm{SOH}_{Q,A}=80\%} \]
For Battery B:
\[ \mathrm{SOH}_{Q,B} = \frac{2.82}{3.00}\times100\% \]
\[ \boxed{\mathrm{SOH}_{Q,B}=94\%} \]
Battery B retains a greater proportion of its original charge capacity.
Part b: Calculate resistance growth
For Battery A:
\[ \%\text{ increase} = \frac{30-25}{25}\times100\% \]
\[ \boxed{20\%} \]
For Battery B:
\[ \%\text{ increase} = \frac{75-25}{25}\times100\% \]
\[ \boxed{200\%} \]
Battery B has experienced considerably greater resistance growth.
Part c: Select the appropriate battery
For the low-power monitoring device, Battery B is the more suitable candidate.
Its higher capacity means it can provide more total charge during operation. Under the assumption that the low current does not cause premature voltage cut-off, capacity is the more important factor for long operating periods.
For the high-power motor, Battery A is the more suitable candidate.
Its lower internal resistance means it experiences less voltage sag when a large current is demanded. It also produces less resistive heating at the same current.
Battery B’s higher capacity does not automatically make it better for high-power applications.
This question demonstrates why battery health cannot always be expressed as a simple ranking.
The best battery depends on what the application requires.
Actual battery selection would also need to consider manufacturer current limits, temperature, safety controls, and the battery management system.
Question 4
A research laboratory investigates electrolyte samples taken from a new and an aged lithium-ion battery.
Equal-volume samples are prepared using the same dilution procedure.
The following observations are recorded:
- Both samples produce a dominant yellow-orange colour in a visual flame test.
- Atomic emission spectroscopy identifies nickel and cobalt in both samples.
- Calibrated AES measurements show higher concentrations of dissolved nickel and cobalt in the aged battery’s electrolyte sample.
- The measured sodium concentrations are similar in both samples.
Answer the following:
a) Explain why the flame test does not provide enough information to distinguish the two samples.
b) Explain why AES provides more useful elemental information.
c) What might the higher dissolved nickel and cobalt concentrations suggest about the aged battery?
d) Explain why these results cannot be used to calculate the battery’s capacity-based SOH or resistance growth. Identify two electrical measurements that would provide more direct information.
Solution 4
The AES results provide evidence of increased transition-metal dissolution in the aged sample, but neither technique directly measures battery state of health.
Part a: Limitation of the flame test
The visual flame test produces a combined visible colour.
The strong yellow-orange emission is consistent with sodium being present in both samples.
However, the human eye cannot reliably separate all the individual emission wavelengths produced by a mixture.
Other elements may be present even if their emissions are not visually distinguishable.
The flame test therefore provides only limited qualitative information about the elemental composition of these samples.
Part b: Advantages of AES
AES separates emitted light into individual wavelengths.
Different elements produce characteristic emission lines, allowing nickel and cobalt to be identified independently of the overall flame colour.
The intensity of the relevant emission lines can then be compared with calibration standards.
This allows their concentrations to be estimated quantitatively.
AES therefore provides much more detailed information about the elemental composition of the samples.
Part c: Interpretation of the increased metal concentrations
The higher concentrations of dissolved nickel and cobalt may indicate increased dissolution of transition metals from the positive electrode material.
This is consistent with chemical degradation of the electrode.
The observation provides evidence of a change in the battery’s internal chemical environment.
However, it does not establish the exact amount of active electrode material that has been lost. A sample of dissolved metals does not provide a complete mass balance of the electrode.
Part d: Why electrical measurements are still needed
Elemental composition and electrical performance are different properties.
The AES results do not tell us how much charge the battery can deliver or how much its internal resistance has increased.
Two more direct measurements are:
- A controlled charge-discharge capacity test, which determines the current usable capacity and allows capacity-based SOH to be calculated.
- A controlled current pulse test, which estimates the battery’s internal resistance under specified conditions.
Electrochemical impedance spectroscopy could provide further information about the battery’s internal electrical response.
The important conclusion is that evidence of chemical degradation is not automatically a numerical measurement of electrical degradation.
Question 5
A lithium-ion battery is being investigated because it performs poorly under high-current conditions.
A new reference cell of the same chemistry originally delivered 3.00 Ah when discharged at 0.30 A and 25 °C, using a specified lower voltage cut-off of 2.80 V.
The aged cell is tested under several conditions.
Test 1: Low-current discharge
When fully charged and discharged at 0.30 A under the same temperature and voltage limits, the aged cell delivers 2.70 Ah.
Test 2: High-current discharge
In a separate fully charged test, the aged cell is discharged at 3.0 A.
It reaches the same 2.80 V cut-off after delivering only 2.10 Ah.
After the discharge current is stopped, the battery rests for 20 minutes. Its terminal voltage recovers to 3.12 V.
The discharge is then resumed at 0.30 A. The cell delivers a further 0.55 Ah before reaching the 2.80 V cut-off again.
Test 3: Resistance measurement
At the same reference state of charge and temperature, a 10-second, 3.0 A current pulse produces the following voltage responses:
| Measurement | New reference cell | Aged cell |
|---|---|---|
| Voltage before pulse | 3.90 V | 3.90 V |
| Voltage after 10 seconds | 3.84 V | 3.74 V |
| Current increase | 3.0 A | 3.0 A |
A technician examines the high-current discharge result and concludes:
“The battery has irreversibly lost 30% of its original chemical capacity because it only delivered 2.10 Ah instead of 3.00 Ah.”
Evaluate this conclusion.
Your response must:
a) Calculate the capacity-based SOH using the low-current reference test.
b) Calculate the total charge delivered during the high-current discharge followed by the lower-current discharge.
c) Calculate the pulse resistance of the new and aged cells and determine the percentage resistance increase.
d) Explain why the battery voltage recovered during the rest period and why additional charge could subsequently be delivered.
e) Evaluate whether the technician’s conclusion is justified. Distinguish between actual capacity loss and the effect of increased resistance on usable capacity under high-current conditions.
Solution 5
The technician’s conclusion is not justified. The low-current test indicates 90% capacity-based SOH, while the pulse test demonstrates substantial resistance growth. The 70% high-current result does not establish a 30% irreversible loss of chemical capacity.
The key is to recognise that the high-current discharge and low-current discharge are not equivalent tests.
Part a: Calculate capacity-based SOH
Use the low-current test because it matches the original reference test conditions.
\[ \mathrm{SOH}_{Q} = \frac{Q_{\mathrm{now}}} {Q_{\mathrm{ref}}} \times100\% \]
Substitute:
\[ = \frac{2.70}{3.00} \times100\% \]
\[ \boxed{\mathrm{SOH}_{Q}=90\%} \]
The measured capacity fade under the reference conditions is:
\[ 100-90=10\% \]
Therefore, the battery retains 90% of its original measured low-rate capacity.
This is the appropriate capacity-based comparison for the specified reference test.
Part b: Calculate the total charge delivered in the staged test
The high-current stage delivers:
\[ Q_1=2.10\ \mathrm{Ah} \]
The lower-current stage delivers:
\[ Q_2=0.55\ \mathrm{Ah} \]
The total charge delivered is:
\[ Q_{\mathrm{total}}=Q_1+Q_2 \]
\[ =2.10+0.55 \]
\[ \boxed{Q_{\mathrm{total}}=2.65\ \mathrm{Ah}} \]
Compare this with the separate low-current result of 2.70 Ah.
The difference is:
\[ 2.70-2.65=0.05\ \mathrm{Ah} \]
The staged test delivers almost the same total charge as the separate low-current test.
This is important evidence that the high-current test stopped before all the charge available under lower-current conditions had been extracted.
Part c: Calculate the pulse resistance
For the new reference cell:
\[ \Delta V_{\mathrm{new}} = 3.90-3.84 \]
\[ \Delta V_{\mathrm{new}}=0.06\ \mathrm{V} \]
Using:
\[ R_{\mathrm{pulse}} = \frac{\Delta V}{\Delta I} \]
\[ R_{\mathrm{new}} = \frac{0.06}{3.0} \]
\[ \boxed{R_{\mathrm{new}}=0.020\ \Omega} \]
For the aged cell:
\[ \Delta V_{\mathrm{aged}} = 3.90-3.74 \]
\[ \Delta V_{\mathrm{aged}}=0.16\ \mathrm{V} \]
Therefore:
\[ R_{\mathrm{aged}} = \frac{0.16}{3.0} \]
\[ \boxed{R_{\mathrm{aged}}=0.0533\ \Omega} \]
Now calculate the percentage resistance increase:
\[ \%\text{ increase} = \frac{R_{\mathrm{aged}}-R_{\mathrm{new}}} {R_{\mathrm{new}}} \times100\% \]
\[ = \frac{0.0533-0.0200}{0.0200} \times100\% \]
\[ \boxed{\text{Resistance increase}\approx167\%} \]
The aged cell has approximately 2.67 times the pulse resistance of the original cell.
This is a substantial increase.
Part d: Explain voltage recovery and additional discharge capacity
The high-current discharge produces a relatively large voltage drop inside the aged cell.
As the cell discharges, the terminal voltage eventually reaches the lower cut-off of 2.80 V.
However, reaching this voltage does not necessarily mean that all the electrochemically available charge has been exhausted.
When the current stops, the immediate ohmic voltage drop disappears.
Over the following rest period, concentration gradients and electrochemical polarisation also relax.
The terminal voltage consequently recovers.
When the battery is discharged again at only 0.30 A, the voltage drop caused by internal resistance is smaller.
The battery can therefore continue delivering charge before its terminal voltage reaches the same lower cut-off.
The additional 0.55 Ah is not newly created charge.
It is charge that remained accessible under the less demanding discharge conditions.
Part e: Evaluate the technician’s conclusion
The technician has confused high-rate deliverable capacity with capacity measured under the original reference conditions.
The high-current test delivers:
\[ \frac{2.10}{3.00}\times100\%=70\% \]
However, this represents the proportion of reference capacity delivered before the voltage cut-off during that particular high-current test.
It is not a direct measurement of the battery’s total remaining capacity.
Three pieces of evidence support this conclusion:
- The low-current test shows 90% capacity retention, rather than 70%.
- The staged discharge delivers 2.65 Ah, close to the 2.70 Ah obtained in the separate low-current test.
- The pulse test shows approximately 167% resistance growth, which provides a strong explanation for the increased voltage sag under high-current conditions.
The most reasonable interpretation is that the battery has experienced both capacity degradation and substantial resistance growth.
The resistance increase makes a significant amount of charge inaccessible under high-current conditions because the voltage reaches the cut-off limit earlier.
However, these measurements cannot establish the exact microscopic degradation mechanism or assign every lost ampere-hour to a particular process.
Additional controlled testing, potentially including electrochemical impedance spectroscopy, would be needed for a more detailed diagnosis.
This is the central lesson of battery state of health: a reduction in charge capacity and an increase in internal resistance describe different aspects of ageing, and one can make the other appear worse under demanding operating conditions.
09Where to take this concept next
Once capacity loss and resistance growth have been identified, the next question is what is happening inside the battery to produce the increased resistance.
Electrochemical impedance spectroscopy (EIS) provides a way to investigate this.
Rather than applying one direct-current pulse, EIS measures how a battery responds to small alternating electrical signals at different frequencies.
Different parts of the response can provide information about ohmic resistance, interfacial processes, and charge-transfer behaviour.
The interpretation requires more advanced models, but the underlying idea follows directly from this article: measuring electrical performance can reveal changes in the chemistry and physical structure of an electrochemical cell.
For the next step, read tutorgum’s Electrochemical Impedance Spectroscopy: Interpreting EIS Data.